Skip to content

A mirco-mechanistic study of oxygen-diffusion crack growth in a Polycrystralline Nickel-based Superalloy

Funding: R: ResearchAward

  • Zhao, Liguo G. (PI)

Engineering and Physical Sciences Research Council: £196,859.00

StatusFinished
Effective start/end date1/10/0730/09/10
Award date8/05/07
Relations