Nanoindentation and adhesion-force-mapping studies of polymer blend films: Factors influencing the measured force of adhesion

Research output: Contribution to conferenceAbstract

Standard

Nanoindentation and adhesion-force-mapping studies of polymer blend films : Factors influencing the measured force of adhesion. / Eaton, P.; Nevell, T. G.; Smart, J. D.; Smith, J. R.; Tsibouklis, J.

2001. Abstract from SCANNING 2001, New York, United States.

Research output: Contribution to conferenceAbstract

Harvard

APA

Vancouver

Author

Bibtex

@conference{451cb7d44c0d4b4899e429cb8b2b6cc6,
title = "Nanoindentation and adhesion-force-mapping studies of polymer blend films: Factors influencing the measured force of adhesion",
author = "P. Eaton and Nevell, {T. G.} and Smart, {J. D.} and Smith, {J. R.} and J. Tsibouklis",
year = "2001",
month = dec,
day = "1",
doi = "10.1002/sca.4950230201",
language = "English",
note = "SCANNING 2001 ; Conference date: 05-05-2001 Through 07-05-2001",

}

RIS

TY - CONF

T1 - Nanoindentation and adhesion-force-mapping studies of polymer blend films

T2 - SCANNING 2001

AU - Eaton, P.

AU - Nevell, T. G.

AU - Smart, J. D.

AU - Smith, J. R.

AU - Tsibouklis, J.

PY - 2001/12/1

Y1 - 2001/12/1

UR - http://www.scopus.com/inward/record.url?scp=33745516114&partnerID=8YFLogxK

U2 - 10.1002/sca.4950230201

DO - 10.1002/sca.4950230201

M3 - Abstract

AN - SCOPUS:33745516114

Y2 - 5 May 2001 through 7 May 2001

ER -

ID: 11659246